Materials: | Er,Cr:YSGG | Chemical Formula: | Y2.93Sc1.43 Ga3.64O12 |
---|---|---|---|
Lattice Constant: | 12.42 | Concentration: | 30 At % (3.7 X 1021 Cm-3 , Dodecahedral Er3+) 2 At % (1.7 X 1020 Cm-3 , Octahedral Cr3+) |
Wavefront Distortion (per Inch Of Rod Length): | 1/2 | Surface Quality: | 10 5 Scratch-dig |
High Light: | laser material,titanium doped sapphire |
Crystal Structure |
Cubic |
Chemical Formula |
Y2.93Sc1.43 Ga3.64O12 |
Lattice Constant |
12.42 |
Concentration |
30 at % (3.7 x 1021 cm-3 , dodecahedral Er3+) |
2 at % (1.7 x 1020 cm-3 , octahedral Cr3+) |
|
Wavefront Distortion (per inch of rod length) |
1/2 |
Surface Quality |
10 5 scratch-dig |
Perpendicularity |
5 ‘ |
Parallelism |
30 |
Barrel Finish |
55 micro-inch ±5 micro-inch |
Chamfer Angle |
45 deg ±5 deg |
Chamfer |
0.005 ±0.003 in |
Length Tolerance |
+0.040 / -0.000 in |
Diameter Tolerance |
+0.0000 / -0.0020 in |
Thermal conductivity(W/mK) |
8 |
Thermal expansion coefficient |
8.1×10-6/K |
Thermo-optical factor(dn/dT)(10-6/K) |
12.3 |
Hardness(Mohs) |
8 |
Density |
5.67g/cm3(Cr&Er doped) |
Sizes, (dia x length), mm |
from 3 x 30 to 12.7 x 127.0 |
Orientation |
<001>, <111> |
Optical and Spectral Properties
Refractive index |
1.92 at 1000nm |
Fluorescent Lifetime |
1400 s |
Emission cross-section, cm2 |
5.2 x 10-21 |
Lasing wavelength, m |
2.791 |
Features
Medical Applications